植物生态与资源

油杉木材物理力学性质研究

  • 曾华浩 ,
  • 肖祥希 ,
  • 高 楠 ,
  • 刘晓辉 ,
  • 陈金章 ,
  • 王丽琴 ,
  • 何文广 ,
  • 连细春 ,
  • 黄声集 ,
  • 黄学敏
展开
  • 1.中南林业科技大学,湖南 长沙 410004;2.福建省林业科学研究院,福建 福州 350012;3.泉州市林业局,福建 泉州362000;4.福建省永春碧卿国有林场,福建 永春 362606;5.永春县林业局,福建 永春 362600
曾华浩,博士研究生,高级工程师,从事景观生态研究。

收稿日期: 2017-08-10

  修回日期: 2017-09-19

  网络出版日期: 2017-12-29

基金资助

福建省省属公益类科研院所基本科研专项(2015R1011-11);国家林业公益性行业科研专项(201304108)

Physico-mechanical Properties of Keteleeria fortunei Wood

  • ZENG Hua-hao ,
  • XIAO Xiang-xi ,
  • GAO Nan ,
  • LIU Xiao-hui ,
  • CHEN Jin-zhang ,
  • WANG Li-qin ,
  • HE Wen-guang ,
  • LIAN Xi-chun ,
  • HUANG Sheng-ji ,
  • HUANG Xue-min
Expand
  • 1.Central South University of Forestry and Technology, Changsha 410004, Hunan China; 2.Fujian Academy of Forestry, Fuzhou 350012, Fujian China; 3.Forestry Bureau of Quanzhou City, Quanzhou 362000, Fujian China; 4.State-owned Forest Farm of Biqing, Yongchun County, Fujian Province, Yongchun 362606, Fujian China; 5.Forestry Bureau of Yongchun Country, Yongchun 362600, Fujian China

Received date: 2017-08-10

  Revised date: 2017-09-19

  Online published: 2017-12-29

摘要

对油杉Keteleeria fortunei木材的物理与力学性质进行测定与比较,结果表明,油杉木材的气干密度为0.576 g·cm-3,全干密度为0.544 g·cm-3,属中密度木材。油杉木材的气干径向、弦向和体积干缩系数分别为4.408%、3.272%和7.892%,气干差异干缩为1.347,油杉木材具有不易开裂和变形的特征。油杉木材的抗弯强度、顺纹抗压强度分别为92.701、57.217 Mpa,端面、弦面和径面硬度分别为4635.9、3420.8和3606.8 N,其抗弯强度、顺纹抗压强度和硬度均属中等。50年生油杉木材的物理力学性质优于22年生马尾松Pinus massoniana、湿地松Pinus elliottii和28年生杉木Cunninghamia lanceolata、秃杉Taiwania cryptomerioides。

本文引用格式

曾华浩 , 肖祥希 , 高 楠 , 刘晓辉 , 陈金章 , 王丽琴 , 何文广 , 连细春 , 黄声集 , 黄学敏 . 油杉木材物理力学性质研究[J]. 亚热带植物科学, 2017 , 46(4) : 347 -350 . DOI: 10.3969/j.issn.1009-7791.2017.04.009

Abstract

The wood physical and mechanical properties of Keteleeria fortunei were determined and compared. The results showed that air-dried density and oven-dry density of the wood were 0.576 g穋m-3 and 0.544 g穋m-3, respectively, which indicated that K. fortunei was medium density wood. The radial, tangential and volume shrinkage coefficients were 4.408%, 3.272% and 7.892%, respectively. And the difference of dry shrinkage was 1.347. The wood of K. fortunei was not easy to crack and deformation characteristics. The bending strength, compression strength parallel to grain, the tangential surface, the radial surface and the surface hardness of K. fortunei wood were 92.701 Mpa, 57.217 Mpa, 4635.9 N, 3420.8 N and 3606.8 N, respectively. The bending strength, compression strength parallel to grain and hardness were all medium. The wood physical and mechanical properties of 50 years old K. fortunei was better than those of 22 year old Pinus massoniana and Pinus elliottii, 28 years old Cunninghamia lanceolata and Taiwania cryptomerioides.

参考文献

[1] 高楠,肖祥希,何文广,郭福泰,陈金章,王丽琴,连细春,黄声集,黄学敏. 50年生油杉人工林生长规律研究[J]. 广西林业科学, 2015,44(3): 219—224.

[2] 高楠,肖祥希,何文广,陈金章,连细春,黄声集,黄学敏. 50年油杉人工林生态系统养分分配格局[J]. 广西林业科学, 2015,44(4): 352—357.

[3] 王丽琴. 福建永春油杉人工林生物量结构特征[J]. 亚热带植物科学, 2015,44(3): 228—230.

[4] 庄奇. 湿地松与马尾松人工林木材物理力学性质的比较研究[J]. 中南林业调查规划, 2004,23(2): 58—59.

[5] 梁宏温,黄恒川,黄承标,黄海仲,梁欣,蒙跃环. 不同树龄秃杉与杉木人工林木材物理力学性质的比较[J]. 浙江林学院学报, 2008,25(2): 137—142.

[6] 林同龙. 乐东拟单性木兰木材物理力学性质的研究[J]. 福建林学院学报, 2011,31(4): 381—384.

[7] 李坚. 木材科学研究[M]. 北京: 科学出版社, 2009.

[8] 赵承开,高建亮,朱林峰,赵林艳. 无性系杉木木材物理性质研究[J]. 中南林学院学报, 2006,26(6): 165—168.

[9] 梁宏温,徐峰,牟继平. 马占相思木材物理力学性质的研究[J]. 广西农业生物科学, 2004,23(4): 325—328.

[10] 陈松武,梁炜文,许彩娟,黄婷,陈晓斌,符韵林. 人工林灰木莲木材物理力学性质研究[J]. 安徽农业科学, 2012,40(16): 8993—8996.

[11] 韦鹏练,黄腾华,符韵林. 观光木人工林木材物理力学性质的研究[J]. 西北林学院学报, 2014,29(6): 221—225.

[12] 黄腾华,符韵林,李宁. 擎天树木材物理力学性质研究[J]. 西北林学院学报, 2013,28(5): 160—163.

[13] 叶忠华,叶友章,刘晓辉,杨淑宝. 毛红椿木材物理力学性质研究[J]. 山地农业生物学报, 2016,35(3): 72—75.

文章导航

/

〈 〉